Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of RADILON S RV300W 333 BK - PA6-GF30 - RadiciGroup High Performance Polymers

Material Data Center offers the following functions for RADILON S RV300W 333 BK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Radilon S datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
PA6 rinforzato 30% fibra vetro per stampaggio a iniezione. Stabilizzato al calore. Colore nero.


Adatto per articoli che richiedono elevata rigidità, buona resistenza meccanica e ottimo mantenimento delle proprietà dopo invecchiamento termico.

Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Ritiro di stampaggio, parallelo 0.3 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.8 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 9400 / 6200 MPa ISO 527
Carico unitario a rottura 165 / 105 MPa ISO 527
Deformazione a rottura 3.2 / 6 % ISO 527
Resistenza all'urto Charpy, +23°C 85 / 100 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 70 / - kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 13 / 20 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 9 / - kJ/m² ISO 179/1eA
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 220 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 200 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 215 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 210 / * °C ISO 306
Coeff.di dilatazione termica lin., parallelo 25 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 95 / * E-6/K ISO 11359-1/-2
Reazione al fuoco a spessore h HB / * class IEC 60695-11-10
Spessore provato 0.8 / * mm -
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Resistività volumica 1E13 / 1E11 Ohm*m IEC 62631-3-1
Resistività superficiale * / 1E10 Ohm IEC 62631-3-2
Res. Alle correnti striscianti superficiali 500 / - - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 7.5 / * % Sim. alla ISO 62
Assorbimento d'umidità 2 / * % Sim. alla ISO 62
Massa volumica 1350 / - kg/m³ ISO 1183
Funzioni
Viscosità-Velocità di taglio , RADILON S RV300W 333 BK, PA6-GF30, RadiciGroup
Sforzo di taglio-Velocità di taglio , RADILON S RV300W 333 BK, PA6-GF30, RadiciGroup
Modulo dinamico a taglio-temperatura , RADILON S RV300W 333 BK (Secco), PA6-GF30, RadiciGroup
Sforzi-deformazione , RADILON S RV300W 333 BK (Secco), PA6-GF30, RadiciGroup
Sforzi-deformazione , RADILON S RV300W 333 BK (cond.), PA6-GF30, RadiciGroup
Modulo secante-deformazione , RADILON S RV300W 333 BK (Secco), PA6-GF30, RadiciGroup
Modulo secante-deformazione , RADILON S RV300W 333 BK (cond.), PA6-GF30, RadiciGroup
Volume specifico-temperatura (pvT) , RADILON S RV300W 333 BK, PA6-GF30, RadiciGroup
Modulo a taglio-temperatura , RADILON S RV300W 333 BK (Secco), PA6-GF30, RadiciGroup
Modulo a taglio-temperatura , RADILON S RV300W 333 BK (cond.), PA6-GF30, RadiciGroup
LTHA-Carico unitario a rottura 4mm, RADILON S RV300W 333 BK, PA6-GF30, RadiciGroup
LTHA-Deformazione a rottura 4mm, RADILON S RV300W 333 BK, PA6-GF30, RadiciGroup
LTHA-Resist. urto Charpy con intaglio (23°C) 4mm, RADILON S RV300W 333 BK, PA6-GF30, RadiciGroup
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Granuli, Nero
Additivi
Agente di distacco
Caratteristiche speciali
Stabilizzato o stabile al calore
Disponibilità geografica
Altre informazioni
Stampaggio ad Iniezione
Il materiale viene consegnato in una confezione a prova di umidità, pronto per la lavorazione. Massimo contenuto di umidità raccomandato per la migliore processabilità pari a 0,15%. Condizioni tipiche del'essiccatore: temperatura 80 °C, punto di rugiada -20 ° C o inferiore, tempo: 2-4 h o più. Durante l'aggiunta di materiale rimacinato, prestare attenzione per evitare l'assorbimento di umidità e la contaminazione con altri polimeri. Possono verificarsi variazioni di colore e riduzione di proprietà meccaniche che devono sempre essere attentamente monitorate.

Stampaggio ad iniezione, Parametri di processo
Temperatura fuso Temperature stampo Velocità iniezione
280 - 300°C80 - 100°Cmedia-alta
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com